DESCRIPTION
Our 5×5 mm CVD polycrystalline diamond substrates are fabricated by MPCVD process, featuring ultra-high thermal conductivity, excellent chemical inertness and mechanical hardness. Available with precision lapped or CMP polished surfaces. Ideal for high-power device thermal spreaders, laser optics, epitaxy research and semiconductor packaging. Custom thickness, surface finish and edge treatment are supported.
- For best experience, create an login when requesting samples.
Specification
| Item | Polycrystalline Diamond Substrate |
| Diameter | 5 x 5mm |
| Thickness | 300mm |
| Surface Finish | Double side polished |
| Surface Orientation | N/A |
| Crystal Growth Method | MPCVD |
| Polish roughness | 1~10nm |
| Thermal Conductivity | >1000 W/m.K |
Customization specifications:
* Various sizes and shapes such as 5*5mm,10*10mm,1~4inch.
* Various thicknesses:0.1~5mm.
* Various surface roughness such as slicing,lapping.
* crystal type:single crystal diamond or polycrystalline diamond.
Properties
| Polycrystalline Diamond Substrate | |
| Crystal Structure | Cubic Crystal |
| Band Gap (eV) | 5.47 eV |
| Melting Point (°C) | 4027 °C |
| Mohs Hardness | 10 |
| Thermal Conductivity (W·cm⁻¹·°C⁻¹) | 20 |
| Thermal Expansion Coefficient (°C⁻¹) | 0.8 × 10⁻⁶ |
| Lattice Constant (nm) | 0.3567 nm |
| Electron Mobility (cm²·V⁻¹·s⁻¹) | 1600 |
| Breakdown Electric Field | 10 |
| JFM Index (Power) | 5330 |
| BFM Index (SW) | 14860 |
| BHFM Index (RF) | 1080 |
| Refractive Index | 2.417 |
Package