DESCRIPTION
Our 4‑inch P‑type <100> Silicon Wafer is monocrystalline silicon substrate manufactured to SEMI specifications. P‑type doped with tight <100> crystal orientation tolerance. Both SSP and DSP surfaces are offered. Custom parameters including resistivity, thickness, TTV and surface flatness are acceptable. Widely applied in thin‑film epitaxy, device development, process verification, MEMS manufacturing and material‑science R&D. Packed in standard wafer carrier against transit damage.
- For best experience, create an login when requesting samples.
Specification
| Item | Silicon Substrate | |
| Diameter | 100.0±0.3mm | |
| Thickness | 500±25μm、1000±25μm、5000±25μm | 100±25μm、500±25μm |
| Surface Finish | Single side polished | Double side polished |
| Surface Orientation | <100> | |
| Crystal Growth Method | CZ | |
| Dopant | P-type (B-Doping) | |
| Primary Flat Length | 32.5±1.0mm | |
| Resistivity | 1~100Ω·cm / <0.01Ω·cm | |
| TTV | ≤10μm | |
| BOW | ≤15μm | |
| WARP | ≤20μm | |
| Edge Exclusion | ≤2 mm | |
Customization specifications:
* Various sizes and shapes such as 10*10mm
* Various thicknesses: 0.1~20mm
* Various surface roughness such as slicing,lapping,polishing.
* Silicon crystal ingots are available.
Properties
| Silicon Substrate | |
| Growth Method | CZ/FZ |
| Crystal Structure | Diamond |
| Lattice Constant(nm) | a=5.4305Å |
| Density(g/cm3) | 2.329 |
| Melting point | 1410°C |
| Mohs Hardness(mohs) | 7 |
| Dielectric Constant | 11.8 |
| Band Gap(eV) | 1.1 |
| Breakdown Electrical Field ((MV/cm)) | 0.3 |
| Thermal Conductivity(n-type) (W/cm.K) | 1.48 |
| Electron Mobility(cm2·V-1·s-1) | 1480 |
| Thermal Expansion | 2.6×10^-6 /°C |
| Refractive Index | 3.5 |
Package