DESCRIPTION
Our 6‑inch P‑type <111> Silicon Wafer is boron‑doped monocrystalline silicon substrate meeting SEMI industry standards. Strictly‑managed <111> crystal orientation deviation. SSP and DSP surface options available. Resistivity, thickness, TTV and global flatness can be adjusted for pilot‑run applications. Extensively used for anisotropic micromachining, MEMS etch‑stop layer processing, bipolar component development, thin‑film epitaxy and advanced sensor research. Securely packed in professional wafer carrier.
- For best experience, create an login when requesting samples.
Specification
| Item | Silicon Substrate |
| Diameter | 150.0±0.3mm |
| Thickness | 625±25μm |
| Surface Finish | Single side polished / Double side polished |
| Surface Orientation | <111> |
| Crystal Growth Method | CZ |
| Dopant | P-type (B-Doping) |
| Primary Flat Length | 47.5±1.0mm |
| Resistivity | 1~100Ω·cm / <0.01Ω·cm |
| TTV | ≤20μm |
| BOW | ≤25μm |
| WARP | ≤30μm |
| Edge Exclusion | ≤2 mm |
Customization specifications:
* Various sizes and shapes such as 10*10mm
* Various thicknesses: 0.1~20mm
* Various surface roughness such as slicing,lapping,polishing.
* Silicon crystal ingots are available.
Properties
| Silicon Substrate | |
| Growth Method | CZ/FZ |
| Crystal Structure | Diamond |
| Lattice Constant(nm) | a=5.4305Å |
| Density(g/cm3) | 2.329 |
| Melting point | 1410°C |
| Mohs Hardness(mohs) | 7 |
| Dielectric Constant | 11.8 |
| Band Gap(eV) | 1.1 |
| Breakdown Electrical Field ((MV/cm)) | 0.3 |
| Thermal Conductivity(n-type) (W/cm.K) | 1.48 |
| Electron Mobility(cm2·V-1·s-1) | 1480 |
| Thermal Expansion | 2.6×10^-6 /°C |
| Refractive Index | 3.5 |
Package