DESCRIPTION
Our 4‑inch P‑type <111> Silicon Wafer is boron‑doped monocrystalline silicon substrate produced to SEMI specifications. Tight tolerance for <111> crystal orientation. Both SSP and DSP polishing versions are offered. Custom parameters including resistivity, thickness, TTV and flatness are acceptable. Widely applied in anisotropic wet‑etching, MEMS fabrication, bipolar device validation, thin‑film growth and sensor‑oriented R&D. Standard wafer carrier packaging prevents mechanical damage during shipment.
- For best experience, create an login when requesting samples.
Specification
| Item | Silicon Substrate |
| Diameter | 100.0±0.3mm |
| Thickness | 500±25μm |
| Surface Finish | Single side polished / Double side polished |
| Surface Orientation | <111> |
| Crystal Growth Method | CZ |
| Dopant | P-type (B-Doping) |
| Primary Flat Length | 32.5±1.0mm |
| Resistivity | 1~100Ω·cm / <0.01Ω·cm |
| TTV | ≤10μm |
| BOW | ≤15μm |
| WARP | ≤20μm |
| Edge Exclusion | ≤2 mm |
Customization specifications:
* Various sizes and shapes such as 10*10mm
* Various thicknesses: 0.1~20mm
* Various surface roughness such as slicing,lapping,polishing.
* Silicon crystal ingots are available.
Properties
| Silicon Substrate | |
| Growth Method | CZ/FZ |
| Crystal Structure | Diamond |
| Lattice Constant(nm) | a=5.4305Å |
| Density(g/cm3) | 2.329 |
| Melting point | 1410°C |
| Mohs Hardness(mohs) | 7 |
| Dielectric Constant | 11.8 |
| Band Gap(eV) | 1.1 |
| Breakdown Electrical Field ((MV/cm)) | 0.3 |
| Thermal Conductivity(n-type) (W/cm.K) | 1.48 |
| Electron Mobility(cm2·V-1·s-1) | 1480 |
| Thermal Expansion | 2.6×10^-6 /°C |
| Refractive Index | 3.5 |
Package