DESCRIPTION
8‑inch thermal‑grown silicon oxide wafer features high‑quality thermally‑formed SiO₂ dielectric layer on monocrystalline silicon substrate. Available in Single‑Side Polished (SSP) and Double‑Side Polished (DSP) with single‑sided or double‑sided thermal oxide. Customizable parameters include oxide thickness, wafer thickness, crystal orientation <100>/<111>, resistivity and doping type (P‑type / N‑type / intrinsic). Suitable for industrial semiconductor process, MEMS device fabrication, photolithography, thin‑film deposition, wafer bonding and advanced laboratory research. Please contact us for detailed specifications and quotation.
- For best experience, create an login when requesting samples.
Specification
| Item | Silicon Substrate |
| Diameter | 200.0±0.3mm |
| Thickness | 725±25μm |
| Oxide layer thickness | 500nm |
| Surface Finish | SSP Single-sided oxide / DSP Double-sided oxide |
| Surface Orientation | <100> |
| Crystal Growth Method | CZ |
| Dopant | N-type / P-type |
| Primary Flat Length | Notch |
| Resistivity | 1~100Ω·cm/<0.01Ω·cm |
| TTV | ≤30μm |
| BOW | ≤40μm |
| WARP | ≤60μm |
| Edge Exclusion | ≤3 mm |
Customization specifications:
* Various sizes and shapes such as 10*10mm
* Various thicknesses: 0.1~20mm
* Various surface roughness such as slicing,lapping,polishing.
* Silicon crystal ingots are available.
Properties
| Silicon Substrate | |
| Crystal Structure | Diamond cubic crystal |
| Band-gap Width (eV) | 1.12 eV |
| Melting Point (°C) | 1414 °C |
| Mohs Hardness | 7 |
| Thermal Conductivity (W·cm⁻¹·°C⁻¹) | 1.5 W·cm⁻¹·°C⁻¹ |
| Thermal Expansion Coefficient (°C⁻¹) | 2.5×10⁻⁶ |
| Lattice Constant (nm) | a=0.5431 |
| Electron Mobility (cm²·V⁻¹·s⁻¹) | 1350 |
| Breakdown Electric Field (MV·cm⁻¹) | 0.3 |
| JFM Index (power) | 1 |
| BFM Index (SW) | 1 |
| BHFM Index (RF) | 1 |
| Refractive Index | 3.5 |
Package