Our 10 x 10 mm CVD Single‑Crystal Diamond Substrate is manufactured via chemical vapor deposition (CVD) method. It features superior thermal conductivity, broad optical transmission range, high hardness and outstanding corrosion resistance.
Customizable options cover substrate thickness, surface condition (as‑grown / polished), crystal orientation and special surface treatment.
This moderate‑size diamond substrate is well‑suited for high‑power laser diode thermal management, RF device packaging, optical window fabrication, quantum material study and laboratory R&D projects.
- For best experience, create an login when requesting samples.
| Item | Single-crystal diamond substrate |
| Diameter | 10 x 10mm |
| Thickness | 100μm、300μm、500μm |
| Surface Finish | Double side polished |
| Surface Orientation | <100> |
| Crystal Growth Method | MPCVD |
| Polish roughness | 1~10nm |
| Thermal Conductivity | 1500-2300W/m.K |
* Various sizes and shapes such as 5*5mm,10*10mm,1~4inch.
* Various thicknesses: 0.1~5mm
* Various surface roughness such as slicing,lapping.
* crystal type:single crystal diamond or polycrystalline diamond.
| Single-crystal diamond substrate | |
| Crystal Structure | Cubic Crystal |
| Band Gap (eV) | 5.47 eV |
| Melting Point (°C) | 4027 °C |
| Mohs Hardness | 10 |
| Thermal Conductivity (W·cm⁻¹·°C⁻¹) | 20 |
| Thermal Expansion Coefficient (°C⁻¹) | 0.8 × 10⁻⁶ |
| Lattice Constant (nm) | 0.3567 nm |
| Electron Mobility (cm²·V⁻¹·s⁻¹) | 1600 |
| Breakdown Electric Field (MV·cm⁻¹) | 10 |
| JFM Index (Power) | 5330 |
| BFM Index (SW) | 14860 |
| BHFM Index (RF) | 1080 |
| Refractive Index | 2.417 |