Our 5 x 5 mm CVD Single‑Crystal Diamond Substrate is synthesized by chemical vapor deposition process. It delivers outstanding thermal conductivity, wide optical transmission range and superior chemical inertness.
Customizable parameters include substrate thickness, surface finish (as‑grown / polished), crystal orientation and surface treatment.
This small‑size diamond substrate is widely used for laser diode heat dissipation, high‑frequency electronic devices, optical windows, quantum material research and university‑level experimental projects.
- For best experience, create an login when requesting samples.
| Item | Single-crystal diamond substrate |
| Diameter | 5 x 5mm |
| Thickness | 500μm |
| Surface Finish | Double side polished |
| Surface Orientation | <100>、<110>、<111> |
| Crystal Growth Method | MPCVD |
| Polish roughness | 1~10nm |
| Thermal Conductivity | 1500-2300W/m.K |
* Various sizes and shapes such as 5*5mm,10*10mm,1~4inch.
* Various thicknesses: 0.1~5mm
* Various surface roughness such as slicing,lapping.
* crystal type:single crystal diamond or polycrystalline diamond.
| Single-crystal diamond substrate | |
| Crystal Structure | Cubic Crystal |
| Band Gap (eV) | 5.47 eV |
| Melting Point (°C) | 4027 °C |
| Mohs Hardness | 10 |
| Thermal Conductivity (W·cm⁻¹·°C⁻¹) | 20 |
| Thermal Expansion Coefficient (°C⁻¹) | 0.8 × 10⁻⁶ |
| Lattice Constant (nm) | 0.3567 nm |
| Electron Mobility (cm²·V⁻¹·s⁻¹) | 1600 |
| Breakdown Electric Field (MV·cm⁻¹) | 10 |
| JFM Index (Power) | 5330 |
| BFM Index (SW) | 14860 |
| BHFM Index (RF) | 1080 |
| Refractive Index | 2.417 |