Our 25 x 25 mm CVD Single‑Crystal Diamond Substrate is grown by chemical vapor deposition. With large effective area, it provides outstanding thermal spreading performance, wide optical transmission and superior mechanical‑chemical stability.
Custom options include substrate thickness, surface finish (as‑grown / polished), crystal orientation and surface modification.
Well‑suited for high‑density power module heat dissipation, large‑aperture optical windows, high‑power laser devices and advanced research projects.
- For best experience, create an login when requesting samples.
| Item | Single-crystal diamond substrate |
| Diameter | 25 x 25mm |
| Thickness | 500μm |
| Surface Finish | Double side polished |
| Surface Orientation | <100> |
| Crystal Growth Method | MPCVD |
| Polish roughness | 1~10nm |
| Thermal Conductivity | 1500-2300W/m.K |
* Various sizes and shapes such as 5*5mm,10*10mm,1~4inch.
* Various thicknesses: 0.1~5mm
* Various surface roughness such as slicing,lapping.
* crystal type:single crystal diamond or polycrystalline diamond.
| Single-crystal diamond substrate | |
| Crystal Structure | Cubic Crystal |
| Band Gap (eV) | 5.47 eV |
| Melting Point (°C) | 4027 °C |
| Mohs Hardness | 10 |
| Thermal Conductivity (W·cm⁻¹·°C⁻¹) | 20 |
| Thermal Expansion Coefficient (°C⁻¹) | 0.8 × 10⁻⁶ |
| Lattice Constant (nm) | 0.3567 nm |
| Electron Mobility (cm²·V⁻¹·s⁻¹) | 1600 |
| Breakdown Electric Field (MV·cm⁻¹) | 10 |
| JFM Index (Power) | 5330 |
| BFM Index (SW) | 14860 |
| BHFM Index (RF) | 1080 |
| Refractive Index | 2.417 |