Our 20 x 20 mm CVD Single‑Crystal Diamond Substrate is synthesized via CVD chemical vapor deposition technology. It combines excellent heat‑spreading capability, broad optical transparency and strong resistance to chemical erosion.
You may customize substrate thickness, surface status (as‑grown / polished), crystal orientation and special surface processing.
Larger usable area makes it perfect for multi‑chip thermal dissipation, high‑power laser components, optical window parts and institutional research projects.
- For best experience, create an login when requesting samples.
| Item | Single-crystal diamond substrate |
| Diameter | 20 x 20mm |
| Thickness | 100μm、300μm、500μm |
| Surface Finish | Double side polished |
| Surface Orientation | <100> |
| Crystal Growth Method | MPCVD |
| Polish roughness | 1~10nm |
| Thermal Conductivity | 1500-2300W/m.K |
* Various sizes and shapes such as 5*5mm,10*10mm,1~4inch.
* Various thicknesses: 0.1~5mm
* Various surface roughness such as slicing,lapping.
* crystal type:single crystal diamond or polycrystalline diamond.
| Single-crystal diamond substrate | |
| Crystal Structure | Cubic Crystal |
| Band Gap (eV) | 5.47 eV |
| Melting Point (°C) | 4027 °C |
| Mohs Hardness | 10 |
| Thermal Conductivity (W·cm⁻¹·°C⁻¹) | 20 |
| Thermal Expansion Coefficient (°C⁻¹) | 0.8 × 10⁻⁶ |
| Lattice Constant (nm) | 0.3567 nm |
| Electron Mobility (cm²·V⁻¹·s⁻¹) | 1600 |
| Breakdown Electric Field (MV·cm⁻¹) | 10 |
| JFM Index (Power) | 5330 |
| BFM Index (SW) | 14860 |
| BHFM Index (RF) | 1080 |
| Refractive Index | 2.417 |