Our 30 x 30 mm CVD Single‑Crystal Diamond Substrate is synthesized by chemical vapor deposition. As large‑area single crystal diamond substrate, it delivers excellent heat spreading capacity, broad optical transmission range, high hardness and corrosion resistance.
Available custom parameters: substrate thickness, surface condition (as‑grown / polished), crystal orientation and special surface treatments.
It is widely adopted for high‑power electronic module thermal management, large‑size optical windows, high‑energy laser equipment and industrial‑grade R&D projects.
- For best experience, create an login when requesting samples.
| Item | Single-crystal diamond substrate |
| Diameter | 30 x 30mm |
| Thickness | 500μm |
| Surface Finish | Double side polished |
| Surface Orientation | <100> |
| Crystal Growth Method | MPCVD |
| Polish roughness | 1~10nm |
| Thermal Conductivity | 1500-2300W/m.K |
* Various sizes and shapes such as 5*5mm,10*10mm,1~4inch.
* Various thicknesses: 0.1~5mm
* Various surface roughness such as slicing,lapping.
* crystal type:single crystal diamond or polycrystalline diamond.
| Single-crystal diamond substrate | |
| Crystal Structure | Cubic Crystal |
| Band Gap (eV) | 5.47 eV |
| Melting Point (°C) | 4027 °C |
| Mohs Hardness | 10 |
| Thermal Conductivity (W·cm⁻¹·°C⁻¹) | 20 |
| Thermal Expansion Coefficient (°C⁻¹) | 0.8 × 10⁻⁶ |
| Lattice Constant (nm) | 0.3567 nm |
| Electron Mobility (cm²·V⁻¹·s⁻¹) | 1600 |
| Breakdown Electric Field (MV·cm⁻¹) | 10 |
| JFM Index (Power) | 5330 |
| BFM Index (SW) | 14860 |
| BHFM Index (RF) | 1080 |
| Refractive Index | 2.417 |